Soft touch film on premium packaging: process notes that decide the result

Velvet surfaces are judged by hand, so small process errors show. Temperature, nip pressure and post-press decoration each change the final feel.

7 min read · 30 Sept 2026

Temperature is the main variable

Soft touch film carries a thicker matting layer than standard matt film, so heat has to travel further before the adhesive flows. Running too cold produces a surface that looks correct and delaminates at the crease two days later.

Run at the upper half of the recommended window and check peel on a cooled sample, not a warm one.

Post-press decoration

Foil stamping on velvet requires more pressure and a slightly higher temperature than on matt film, because the textured surface does not contact the foil evenly. Embossing depth is limited by the same texture.

Handling after lamination

Velvet surfaces hold oils. If cartons are stacked immediately after gluing, the film can pick up marks from handlers. Anti-fingerprint grades reduce this; gloves and a short settling period help further.

Before you commit a roll

Trial on your own board at production speed. Send the substrate, ink coverage and machine model and we will confirm a starting grade and temperature.

Ask about this application

Enquiry

Tell us what you laminate.

Board weight, ink coverage, film gauge and machine model are enough to start. We reply with a grade suggestion and a starting temperature for your trial.

Company
Xiamen Zchain Industry Co., Ltd.
Location
Xiamen, Fujian, China

Distributors and OEM label projects: mention your market and annual volume and we will route the enquiry accordingly.

+86 159 5920 0670

Request a Free Sample